Suzhou Crystal Base New Materials Co.,Ltd
Welcome Visitors to Booth No. 1146 GlassBuild America Oct.19-21,2016 Las Vegas Nevada,USA
Place of Origin: | China |
Brand Name: | Crystal Base |
Certification: | CE/CSI/BS/ASTM |
Model Number: | TSG |
Minimum Order Quantity: | 100sqm |
---|---|
Price: | negotiation |
Packaging Details: | Packed in Strong Plywood Crates or Cases with PE,paper or Saftpad interlayer |
Delivery Time: | 15 days after order confirmed |
Payment Terms: | T/T ,L/C,DP or western Union |
Supply Ability: | 3,000 Sqm per Day |
Product Name: | Tempered Safety Glass | Application: | Home Appliance Glass Panels |
---|---|---|---|
Size Of Panel: | Various | Colours: | Clear, Blue, Gray, Brown. |
Standard: | CE/CSI/BS/ASTM | Type: | Flat Or Curved Sheet Glass |
Thickness: | 2-19mm | Transmittance: | More Than 88% |
High Light: | tempered float glass,toughened safety glass |
Low Iron Custom Tempered Glass Panels , Laminated Glass Film Safety
Specification:
|
Description
The laminated glass is one kind of safety glass made under high temperature by interlaying PVB
membrane between glasses. It can be two sheets or more than two sheets.
The firm and tough bindings between PVB films and the glass makes laminated glass the safe
glass with excellent performance. Vertically or sideling installed, it can resist the external impact
and prevent penetration. Once broken, the broken pieces will still be stuck with the middle coatings
so as to avoid human injury or property loss because of glass falling. Moreover, the whole glass
still keeps its integrity and can continue to resist impact and provide a shelter from wind and rain.
Tempered glass production process
1. Cutting : cutting the annealing glass to the actual needs of shape.
2. Glass edging: Edging machine to mill the four edges to prevent frund when steeling,while
maintaining the beautiful appearance.
3. Drilling hole:If need to drilling hole using drilling machine.
4. Washing dry:cleaning the glass with washing maching.
5. Tempered glass:Tempered glass is produced by heating annealed glass in a furnace to 700°,
then the glass is rapidly cooled with jets of cold air to 40°,through the procedures, the original
glass is formed of tempered glass.